Determination of the optical GAP in thin films of amorphous dilithium phthalocyanine using the Tauc and Cody models
- María Elena Sánchez-Vergara(corresponding author),
- Juan Carlos Alonso-Huitron,
- Arturo Rodriguez-Gómez,
- Jerry N. Reider-Burstin
- ,
- ,
- Universidad Nacional Autónoma de México,
- Universidad Anáhuac
Open access
Publication Information
Output type
Original language
EnglishPages from-to (Number of pages)
Pages 10000-10013 (14 pages)Journal (Volume, Issue Number)
Molecules (Volume 17, Issue 9)Publication milestones
- Published - 01/09/2012
Publication status
Publication IDs
- Scopus: 84866944662
- PubMed: 22922272
Abstract
Semiconducting thin films were grown on quartz substrates and crystalline silicon wafers, using dilithium phthalocyanine and the organic ligands 2,6-dihydroxyanthraquinone and 2,6-diaminoanthraquinone as the starting compounds. The films, thus obtained, were characterized by Fourier Transform infrared (FTIR), fast atomic bombardment (FAB+) mass and ultraviolet-visible (UV-Vis) spectroscopies. The surface morphology of these films was analyzed by means of atomic force microscopy (AFM) and scanning electron microscopy (SEM). It was found that the temperature-dependent electric current in all cases showed a semiconductor behavior with conductivities on the order of 10 -6·S cm -1, whereas the highest value corresponded to the thin film based upon the bidentate amine. The Tauc and Cody optical band gap values of thin films were calculated from the absorption coefficients and were found to be around 1.5 eV, with another strong band between 2.3 and 2.43 eV, arising from non-direct transitions. The curvature in the Tauc plot influencing the determination of the optical gap, the Tauc optical gap corresponding to the thicker film is smaller. The dependence of the Cody optical gap on the film thickness was negligible.