Study of prolonged light-soaking (∼400 Hrs) effect on Pm-Si:H solar cell structures
- L. Hamui(autor correspondiente),
- B. M. Monroy,
- G. Santana,
- M. Lopez-Lopez,
- P. Roca Cabarrocas
- Universidad Nacional Autónoma de México,
- Centro de Investigacion y de Estudios Avanzados del Instituto Politécnico Nacional,
- Laboratoire de Physique des Interfaces et des Couches Minces
Producción científica:
Capítulo del libro/informe/acta de congreso
Contribución a la conferencia
Investigación
Revisión por expertosPublication Information
Tipo de resultado
Producción científica:
Capítulo del libro/informe/acta de congreso
Contribución a la conferencia
Investigación
Revisión por expertosIdioma original
InglésNúmero de artículo
7356307Hitos de publicación
- Publicada - 14/12/2015
Estado de publicación
Publicada - 14/12/2015
Editorial
Institute of Electrical and Electronics Engineers Inc.Serie de publicación
- Nombre de serie de publicación: 2015 IEEE 42nd Photovoltaic Specialist Conference, PVSC 2015
ISBN (electrónico)
9781479979448ID de publicación
- Scopus: 84961666271
Título de publicación principal
2015 IEEE 42nd Photovoltaic Specialist Conference, PVSC 2015Abstract
<p>Different pm-Si:H structures were grown using PECVD technique in order to study the effect of light exposition on solar cell structures based on these materials. PIN and NIP structures were analyzed during 400 hrs of light-soaking exposition. The evolution of the structural and optical properties was observed and characterized by Raman spectroscopy, spectroscopic ellipsometry and exodiffusion experiments. The effect observed is related to defects creation due to induced hydrogen diffusion, break of Si-H bonds and the generation of dangling bonds that causes less passivated films. The film microstructure, hydrogen stability, configuration and therefore the optical properties varied with the exposition time. The crystalline fraction of these structures is between 12 to 18% and increase with the exposition time. The optical gap decreases from 1.76 to 1.6 eV for the PIN structure while for the NIP decreases from 1.62 to 1.54 eV. The hydrogen stability and its amount bonded in these films are dependent of the device architecture. Hydrogen diffusion induces structural crystallization and generates a decrease on the absorption properties of the films which in turn is expected to reduce the device efficiency during operation. In this work we show that long range motion of hydrogen during light soaking causes a hydrogen rearrangement on the film and microstructure changes along with a shift on the exodiffusion peaks. Hydrogen diffusion is very different during light-soaking for both structures. We determined that the total hydrogen that effuses from PIN structure is lower than for the NIP, which is expected to cause less degradation of its optoelectronic properties under illumination, and a more stable device during operation.</p>
Publication metrics
PlumX, se abre en una pestaña nueva
Capturas
4